Coating formula: new modified ammonium polyphosphate fire retardant coating formula
-
Last Update: 2020-04-03
-
Source: Internet
-
Author: User
Search more information of high quality chemicals, good prices and reliable suppliers, visit
www.echemi.com
Core tips: 1 Modified ammonium polyphosphate fire retardant coating formulation: raw material quality content /% emulsion 20 ~ 30APP20 ~ 25PER5 ~ 15MEL5 ~ 15 titanium white powder 2~5 filler 2~5 water 20~30 various auxiliaries 2, performance: excellent fire retardant performance, and decoration, non-toxic, pollution-free and environment-friendly characteristics 3 Preparation process of coating: add water, flame retardant, titanium dioxide and various additives in sequence according to the formula, stir for 15min at high speed of 800-1000r / min, sand for 2h, and mix the slurry at 200-4 Which is the price of Dajin diatom mud Recommended brief introduction: which is the price of Dajin diatom mud? How to buy genuine diatom mud? Guangdong diatom mud agent suggests placing a basin of cold water in the air conditioning room, so that the diatom mud wall can breathe effectively The feature of the breathing wall is obvious When the indoor air is dry, the diatom mud wall will release the absorbed water quickly Put it out to help regulate the indoor dry humidity It is suggested to place a basin of cold water in the air conditioning room, so that the wall of diatom mud can breathe effectively The feature of the wall that can breathe is obvious When the indoor air is relatively dry, the wall of diatom mud will absorb the water Coatings home news: 1, modified ammonium polyphosphate fire retardant coating formulation: raw material quality content /% emulsion 20~30 APP 20~25 PER 5~15 MEL 5~15 titanium white 2~5 filler 2~5 water 20~30 various auxiliaries 2, performance: excellent fire resistance, and has decorative, non-toxic, pollution-free and environmentally friendly features 3, the preparation process of paint: add water, flame retardants, titanium dioxide and various auxiliaries in accordance with the formula, stir 15min at high speed 800 ~ 1000r/min, sanding 2h, add slurry additives at 200 to 400r/min, and then paint at low speed (the paint formula in this paper is for reference only) paint home is focused on the news and information of coating, diatom mud, paint coating, coating process, fire retardant coating, and coating, diatom mud, paint coating, coating process, decoration knowledge and decoration effect map of fire retardant coating,
This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only.
This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of
the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed
description of the concern or complaint, to
service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content
will be removed immediately.