    Core tips: 1 The reference formula of conductive coating is as follows: S / N component dosage 1 stainless steel ball (particle size 1mm) 5002 tin oxide (average particle size 0.2um) 383 MEK 704 isopropanol 305 organic silicon strong coating solvent solution (Daicel cr-coati, solid content 30%) 100 2 process The above components are put into a metal container, stirred by a variable speed mixer, mixed and dispersed for 6h to obtain a conductive coating 3 performance The coating can be applied by conventional method After the coating is air dried, the temperature is 80 ℃ Paint agent, top 10 Chinese wall paint brands Recommended introduction: interior wall paint and exterior wall paint can achieve beautiful, clean and pleasant effects, but the effects in different environments are different, so the color of the paint will be different There are ten brands of Chinese paint, ten brands of global paint, ten brands of Chinese wall paint, and ten brands of Chinese paint, Famous trademark of Chinese paint and coating In private rooms, most of us choose according to our own personality, personal hobbies and living habits The younger generation will choose the interior wall paint with rich colors and bright colors, while the older ones will have some working experience Coating home news: 1 The reference formula of conductive coating is as follows: No component dosage 1 stainless steel ball (particle size 1mm) 500 2 tin oxide (average particle size 0.2um) containing antimony trioxide 38 3methyl ketone (MEK) 70 4 isopropanol 30 5 organic silicon strong coating solvent solution (daicelcr-coati, solid content 30%) 100 2 Process The above components are put into a metal container, stirred by a variable speed mixer, mixed and dispersed for 6h to obtain a conductive coating 3 The coating can be coated by conventional method After the coating is air dried, it is dried at 80 ℃ for 4h, and the dry film thickness is 2 μ M The coating has good adhesion to plastic substrate, transparency, scratch resistance and solvent resistance, and can maintain long-term and stable conductivity 4 Application the coating is used in the fields of electronic devices, motor parts, and floors and walls of semiconductor factories (the proportion of each raw material is the number of quality parts) coating house is specialized in coating, diatom mud, paint coating, coating process, news information and coating of fireproof coating, diatom mud, paint coating, coating process, decoration knowledge and decoration effect map of fireproof coating,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.