    Coating formula: reference formula of fine art texture powder coating

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Key tips: 1 Base powder formula Component name: quality: epoxy resin 551.2 curing agent 29.0 carbon black 0.4 titanium dioxide 401.5 iron red 0.4 iron yellow 9.5 benzoin 8.0 2 Bottom powder manufacturing process The above components are stirred and mixed at high speed, then melted and mixed by extruder, cooled, pressed and roughly broken, and finally ground, graded and screened by ACM grinder to obtain qualified bottom powder Process control: material temperature 90 ~ 100 ℃ 3 Formula of mixed powder Name of component: quality of base powder: 98.0 ~ 99.5; texture agent: 0.5 Which is the price of Dajin diatom mud Recommended brief introduction: which is the price of Dajin diatom mud? How to buy genuine diatom mud? Guangdong diatom mud agent suggests placing a basin of cold water in the air conditioning room, so that the diatom mud wall can breathe effectively The feature of the breathing wall is obvious When the indoor air is dry, the diatom mud wall will release the absorbed water quickly Put it out to help regulate the indoor dry humidity It is suggested to place a basin of cold water in the air conditioning room, so that the wall of diatom mud can breathe effectively The feature of the wall that can breathe is obvious When the indoor air is relatively dry, the wall of diatom mud will absorb the water Home of coatings: 1 Formula name of base powder: quality: epoxy resin 551.2 curing agent 29.0 carbon black 0.4 titanium dioxide 401.5 iron red 0.4 iron yellow 9.5 benzoin 8.0 2 Manufacturing process of base powder The above components are stirred and mixed at high speed, then melted and mixed by extruder, cooled, pressed and roughly broken, and finally ground, graded and screened by ACM grinder to obtain qualified bottom powder Process control: material temperature 90 ~ 100 ℃ 3 Formula name of the mixed powder, quality content, bottom powder, 98.0 ~ 99.5, texture agent, 0.5 ~ 2.04 In the manufacturing process of the mixed powder, mix all components of the mixed powder formula in the inverted cone mixer (low shear), mix for 10 ~ 30min, and then discharge the mixture evenly 5 Main performance curing conditions: 200 ℃, 10min; 180 ℃, 15min; 160 ℃, 20min, coating thickness: 63.5 μ M 6 Purpose filing cabinet, high and low voltage distribution cabinet, household appliances, oven, crowbar door, etc Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.