    Key tips: 1 Acrylic Metallic paint formula: The amount of coating material / kgmetaiiux1615.5 acrylic resin 70.5cab-551-0.22.5 dispersant 0.2 leveling agent appropriate amount of anti settling agent appropriate amount of solvent appropriate amount of various colors of organic pigment appropriate amount 2 Acrylic metal paint production process: (1) Prepare raw materials according to the paint formula; (2) Aluminum powder was slowly added into the resin solution for 300r / min and stirred for 30min; (3) Adding "transparent color paste & Rd" under stirring Which is the price of Dajin diatom mud Recommended brief introduction: which is the price of Dajin diatom mud? How to buy genuine diatom mud? Guangdong diatom mud agent suggests placing a basin of cold water in the air conditioning room, so that the diatom mud wall can breathe effectively The feature of the breathing wall is obvious When the indoor air is dry, the diatom mud wall will release the absorbed water quickly Put it out to help regulate the indoor dry humidity It is suggested to place a basin of cold water in the air conditioning room, so that the wall of diatom mud can breathe effectively The feature of the wall that can breathe is obvious When the indoor air is relatively dry, the wall of diatom mud will absorb the water Paint Home News: 1 Acrylic metal paint formula: paint raw material amount / kgme taiiux1615.5 acrylic resin 70.5cab-551-0.22.5 dispersant 0.2 leveling agent amount anti sedimentation agent amount solvent amount organic pigment amount 2 Acrylic metal paint production process: (1) prepare raw materials according to paint formula amount; (2) Add aluminum powder into resin solution slowly under stirring for 300r / min, stirring for 30min; (3) add "transparent color paste" under stirring for color mixing, add resin, solvent, auxiliary agent for 300r / min, stirring for 30min; (4) grind until the fineness is qualified, reduce the speed, stir evenly, adjust the viscosity, filter; (5) discharge, load the barrel, and put into storage Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.