    Core tips: 1 Coating formula: raw material amount / kg raw material amount / kg sodium hydroxide 1.7 light calcium carbonate powder 40 cellulose 3.3 heavy calcium carbonate powder 75 sodium benzoate 0.6600 mesh talcum powder 100 polyvinyl alcohol 38 borax 0.2 cellulose 50 calcium ash powder 60 whitening agent 0.15 ultramarine 0.15 pearl powder 0.15 dibutyl alcohol 0.08 sodium silicate 5 glycol 0.08 thickener 0.5 thickener 0.5 proper amount of water 2 Coating production process: (1) Take 100kg water, add 7kg corn starch, and then Application scope and advantages of roller ceramic coating Recommended introduction: the surface of ceramic rubber plate used for roller ceramic coating is cast into durable rubber plate by hundreds of independent small ceramic pieces Each ceramic piece has raised characteristics Under general conveyor belt pressure, thousands of unique cast bumps can produce positive traction, prevent slipping and extend the service life of conveyor belt roller At the same time, the bottom layer adopts high-quality rubber, which has strong elasticity and can play a good impact resistance role The scope of application of roller ceramic coating is one three six 83857180 (the same as V) 1 Roller coating in extremely harsh working environment 2 The belt joint is not suitable for fixing with iron buckle; 3 It is suitable for leather Home of coatings: 1 Coating formula: raw material amount / kg raw material amount / kg sodium hydroxide 1.7 light calcium carbonate powder 40 cellulose 3.3 heavy calcium carbonate powder 75 sodium benzoate 0.6600 mesh talcum powder 100 polyvinyl alcohol 38 borax 0.2 cellulose 50 calcium ash powder 60 whitening agent 0.15 ultramarine 0.15 pearlescent powder 0.15 dibutyl alcohol 0.08 sodium silicate 5 glycol 0.08 thickener 0.5 thickener 0.5 appropriate amount of water 2 Coating production process: (1) take 100kg of water and add 7kg of corn starch, then add 1.7kg of sodium hydroxide dissolved in a little water, and put it into the mixer to mix to make corn starch gum (2) Take 100kg of water, add 3.3kg of cellulose and 0.6kg of sodium benzoate, and mix them in a mixer to make cellulose glue (3) Heat 100kg of water to 100 ℃, add 3.8kg of polyvinyl alcohol and 0.2kg of borax, and boil to make polyvinyl alcohol glue (4) Take 75kg of polyvinyl alcohol glue, add 60kg of lime powder, 40kg of light calcium carbonate powder, 75kg of heavy calcium carbonate powder and 100kg of 600 mesh talcum powder, mix them in the mixer, add 75kg of corn starch glue while stirring, and then add 50kg of cellulose, and continue to mix them into paste (5) Add 0.15kg of whitening agent and 0.15kg of Ultramarine to the paste, add 0.08kg of dibutyl alcohol and 0.08kg of glycol, add 0.5kg of thickening agent and 0.15kg of pearlescent powder, mix well, then add 5kg of sodium silicate, mix well, finally add 0.5kg of thickening agent, mix well, make the thick paste, grind the thick paste, seal and pack it to form the product 3 Performance: non toxic and tasteless, no pollution and pollution to the environment, smooth and hard scratch coating, smooth and bright, strong adhesion Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.