    Coating process: production process of polyester polyurethane optical fiber coating

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Core tips: production process: The coating formula of polyester type polyurethane optical fiber coating is as follows: Paint Institute → paint formula → paint formula of polyester polyurethane optical fiber coating The production process of polyester polyurethane optical fiber coating is as follows: Poly (tetramethylene ether glycol) reacted with toluene diisocyanate at 70 ℃ for 2 h, then hydroxyethyl acrylate was added, and then reacted at 70 ℃ for 2 h, then cooled to get oligomer Add isodecyl acrylate and benzyldimethylketal and stir well Which is the price of Dajin diatom mud Recommended brief introduction: which is the price of Dajin diatom mud? How to buy genuine diatom mud? Guangdong diatom mud agent suggests placing a basin of cold water in the air conditioning room, so that the diatom mud wall can breathe effectively The feature of the breathing wall is obvious When the indoor air is dry, the diatom mud wall will release the absorbed water quickly Put it out to help regulate the indoor dry humidity It is suggested to place a basin of cold water in the air conditioning room, so that the wall of diatom mud can breathe effectively The feature of the wall that can breathe is obvious When the indoor air is relatively dry, the wall of diatom mud will absorb the water Home of coatings: production process: for the coating formula of polyester polyurethane optical fiber coating, please refer to the following contents: → coating College → coating formula → coating formula of polyester polyurethane optical fiber coating production process of polyester polyurethane optical fiber coating is as follows: the reaction of polyethylene tetramethylene ether glycol and toluene diisocyanate at 70 ℃ 2 h Then hydroxyethyl acrylate was added and reacted at 70 ℃ for 2 h, then cooled to get oligomer The polyester type polyurethane optical fiber coating was prepared by adding isodecyl acrylate and benzyl Dimethylketal and stirring well Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.