Coating process: production process of vinyl acetate acrylate emulsion paint
-
Last Update: 2020-04-03
-
Source: Internet
-
Author: User
Search more information of high quality chemicals, good prices and reliable suppliers, visit
www.echemi.com
Key tips: 1 Production formula of vinyl acetate acrylate emulsion paint Emulsion paint component dosage / kg water 470 dispersant 5 surfactant 1.5 defoamer 3 glycol 25 rutile titanium dioxide 120 silica powder 40 calcium carbonate 100 fibrous talc 150 phenylmercury acetate 0.3 diethylene glycol ether acetic acid solution 8 surfactant 1.5 vinyl acetate acrylate copolymer 2002, vinyl acetate acrylate emulsion paint production process (1) Add 190kg water Paint knowledge | precautions for wall paint color selection Recommended introduction: when painting the wall, the owner sometimes has difficulty in choosing what color of the wall paint to paint In fact, there is no ugly color in the wall paint, only the disharmonious color matching The use of wall color contains the knowledge of health Too strong color will stimulate people's perception, make people have a sense of fidgety, affect people's mental health Grasp the basic principles of wall color and paint a colorful space 1、 Wall paint color selection notice 1 Light color is generally used for the top surface Light colors make people feel light, dark colors make people feel heavy Usually, the treatment of rooms is from top to bottom, from shallow to deep For example, the ceiling and walls of rooms are white and Paint House News: 1 Production formula of vinyl acetate acrylate emulsion paint Emulsion paint component dosage / kg water 470 dispersant 5 surfactant 1.5 defoamer 3 glycol 25 rutile titanium dioxide 120 silica powder 40 calcium carbonate 100 fibrous talc 150 phenylmercury acetate 0.3 diethylene glycol ether acetic acid solution 8 surfactant 1.5 vinyl acetate acrylate copolymer 2002, vinyl acetate acrylate emulsion paint production process (1) Add 190kg water into the cylinder of the disperser, start the mixer, add 1.5kg dispersant, surfactant, defoamer, glycol, titanium dioxide, silica powder, calcium carbonate, and fibrotalc, disperse at high speed for 15min (4900r / min), make them fully dissolved and mix evenly; (3) Check that the fineness is 4.5, add phenylmercury acetate, diethylene glycol ether acetic acid solution, vinyl acetate acrylate copolymer, surfactant 1.5kg and residual water, mix evenly at low speed; (4) stop the machine, discharge and load the barrel, close the barrel cover tightly, and get the finished product Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only.
This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of
the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed
description of the concern or complaint, to
service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content
will be removed immediately.