Coating process: production process of vinyl acetate alkyl maleic acid butyl ester interior gloss emulsion paint
-
Last Update: 2020-04-03
-
Source: Internet
-
Author: User
Search more information of high quality chemicals, good prices and reliable suppliers, visit
www.echemi.com
The key points are as follows: 1 The amount of raw materials for the formulation paint of vinyl acetate alkylmaleate butyl ester / kg, thickener 220, surfactant 6, dispersant 5, glycol 20, preservative 0.3, rutile titanium dioxide 150, silica powder 30, aluminum silicate 100, mica 125, water 280, diethylene glycol monoethyl ether acetate 9, defoamer 2, vinyl acetate alkylmaleate 1752, vinyl acetate alkylmaleate butyl ester Production process of interior gloss emulsion paint: (1) Prepare the raw materials according to the emulsion paint formula; (2) Add surfactant, titanium dioxide, silicon powder, 75kg thickener Paint agent, top 10 Chinese wall paint brands Recommended introduction: interior wall paint and exterior wall paint can achieve beautiful, clean and pleasant effects, but the effects in different environments are different, so the color of the paint will be different There are ten brands of Chinese paint, ten brands of global paint, ten brands of Chinese wall paint, and ten brands of Chinese paint, Famous trademark of Chinese paint and coating In private rooms, most of us choose according to our own personality, personal hobbies and living habits The younger generation will choose the interior wall paint with rich colors and bright colors, while the older ones will have some working experience Paint House News: 1 Formulation of vinyl acetate alkyl maleate butyl ester interior gloss emulsion paint Coating raw material amount / kg thickener 220 surfactant 6 dispersant 5 glycol 20 preservative 0.3 rutile titanium dioxide 150 silicon powder 30 aluminum silicate 100 mica 125 water 280 diethylene glycol monoethyl ether acetate 9 defoamer 2 vinyl acetate alkylmaleate 1752, vinyl acetate alkylmaleate butyl ester internal gloss emulsion paint production process: (1) Prepare the raw materials according to the above emulsion paint formula; (2) add surfactant, titanium dioxide, silicon powder, 75kg thickener, dispersant, preservative, aluminum silicate, mica and water into the paint mixing barrel, start the mixer to mix (high-speed dispersion, 1000r / min) until the fineness is qualified; (3) Reduce the speed (300r / min ~ 400R / min) and further add the remaining components in the emulsion paint formula, mix and mix evenly; (4) use chemical pump to input the mixed emulsion paint into the grinder, grind to the required fineness, discharge, filter, barrel and storage Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only.
This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of
the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed
description of the concern or complaint, to
service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content
will be removed immediately.