    Coating process: production process of water-based steel plate colored primer

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Core tips: 1 Formulation of waterborne steel plate colored primer: formulation dosage / kg dispersant 14.81 defoamer 1.32 surfactant 3.48 water 154.59 iron red 101.57 lead-free white pigment 122.78 talcum powder 46.48 fine barite powder 62.24 acrylic resin 455.25 wetting agent 10.94 n-propoxyethanol 66.92 glycol 9.56 dibutyl phthalate 9.56 preservative 15.122, production process of waterborne steel plate colored primer : (1) Prepare raw materials according to the paint formula; (2) will Paint agent, top 10 Chinese wall paint brands Recommended introduction: interior wall paint and exterior wall paint can achieve beautiful, clean and pleasant effects, but the effects in different environments are different, so the color of the paint will be different There are ten brands of Chinese paint, ten brands of global paint, ten brands of Chinese wall paint, and ten brands of Chinese paint, Famous trademark of Chinese paint and coating In private rooms, most of us choose according to our own personality, personal hobbies and living habits The younger generation will choose the interior wall paint with rich colors and bright colors, while the older ones will have some working experience Home of coatings: 1 Formulation of waterborne steel plate colored primer: formulation dosage / kg dispersant 14.81 defoamer 1.32 surfactant 3.48 water 154.59 iron red 101.57 lead-free white pigment 122.78 talcum powder 46.48 fine barite powder 62.24 acrylic resin 455.25 wetting agent 10.94 n-propoxyethanol 66.92 glycol 9.56 dibutyl phthalate 9.56 preservative 15.122 production process of waterborne steel plate colored primer: (1) prepare raw materials according to the coating formula; (2) Add 103.33kg water into the pull cylinder of the paint dispersion mixer, start the mixer (rotating speed: 300r / min), slowly add dispersant, defoamer, surfactant, iron red, lead-free white pigment, talcum powder and fine barite powder in turn and mix evenly; (3) increase the mixer speed to more than 1000r / min and mix for 20-30 minutes; (4) After the fineness is qualified, reduce the speed and adjust the viscosity to 380MPa · s; (5) shut down, filter, discharge, barrel and store Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.