    Coating process: production process of water diluted air dry alkyd yellow primer

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Core tips: 1 Formulation of water diluted air dry alkyd yellow primer: formulation dosage / kg of water diluted alkyd 221.9 glycol butyl ether 45.7 dispersant 1.1 water 421.9 ammonia water 15.6 calcium carbonate 63.3 barium white 126.6 iron yellow 87.7 zinc phosphate 63.3 silica (amorphous) 21.1 silica (thermolysis) 6.3 black pigment 0.3 glycol monomethyl ether 15.0 cobalt dry material 1.1 calcium dry material 3.2 zirconium dry material 1.5 drier 12 Production process of water dilution air dry alkyd yellow primer: Paint agent, top 10 Chinese wall paint brands Recommended introduction: interior wall paint and exterior wall paint can achieve beautiful, clean and pleasant effects, but the effects in different environments are different, so the color of the paint will be different There are ten brands of Chinese paint, ten brands of global paint, ten brands of Chinese wall paint, and ten brands of Chinese paint, Famous trademark of Chinese paint and coating In private rooms, most of us choose according to our own personality, personal hobbies and living habits The younger generation will choose the interior wall paint with rich colors and bright colors, while the older ones will have some working experience Home of coatings: 1 Water diluted air dry alkyd yellow primer formula: paint formula dosage / kg water diluted alkyd 221.9 glycol butyl ether 45.7 dispersant 1.1 water 421.9 ammonia water 15.6 calcium carbonate 63.3 barium white 126.6 iron yellow 87.7 zinc phosphate 63.3 silica (amorphous) 21.1 silica (pyrolysis) 6.3 black pigment 0.3 ethylene glycol monomethyl ether 15.0 cobalt dry material 1.1 calcium dry material 3.2 zirconium dry material 1.5 drier 12 Water dilution air dry alkyd yellow primer production process: (1) prepare raw materials according to the paint formula; (2) Add 150.8kg water diluted alkyd into the pull cylinder of the paint dispersion mixer, start the mixer (rotating speed: 300r / min), slowly add glycol butyl ether, dispersant, 11.4kg ammonia water, 247.9kg, pigment and filler in turn and mix evenly; (3) increase the mixer rotating speed to 1000r / min and disperse to 7.5ns; (4) Reduce the speed, add the remaining components, adjust the viscosity to be qualified, and mix evenly; (5) stop the machine, filter, discharge, barrel and store in the warehouse Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.