    Coating process: production process of waterborne amino acid white enamel

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    The key points are as follows: 1 Formulation of water-based amino acid white enamel: raw material dosage / kg, short oil degree, water-based alkyd resin 259.3 melamine resin 25.9 triethylamine 16.1 glycol monobutyl ether 77.6 anti shrinkage agent 1 titanium dioxide 200.6 water 409.72, production process of water-based amino acid white enamel: (1) Prepare raw materials according to the paint formula; (2) 146.2kg short oil waterborne alkyd resin was added into the pull cylinder of the paint dispersion mixer, the mixer was started (rotating speed: 300r / min), and then melamine resin and 7 Paint agent, top 10 Chinese wall paint brands Recommended introduction: interior wall paint and exterior wall paint can achieve beautiful, clean and pleasant effects, but the effects in different environments are different, so the color of the paint will be different There are ten brands of Chinese paint, ten brands of global paint, ten brands of Chinese wall paint, and ten brands of Chinese paint, Famous trademark of Chinese paint and coating In private rooms, most of us choose according to our own personality, personal hobbies and living habits The younger generation will choose the interior wall paint with rich colors and bright colors, while the older ones will have some working experience Home of coatings: 1 Formula of water-based amino acid white enamel: raw material consumption / kg, short oil degree, water-based alkyd resin 259.3, melamine resin 25.9, triethylamine 16.1, glycol monobutyl ether 77.6, anti shrinkage agent 1, titanium dioxide 200.6, water 409.7 2, production process of water-based amino acid white enamel: (1) prepare raw materials according to the formula; (2) 146.2kg of short oil waterborne alkyd resin was added to the pull cylinder of the paint dispersion mixer, the mixer was started (rotating speed: 300r / min), and then melamine resin, 7.6kg triethylamine, glycol monobutyl ether, shrinkage agent and titanium dioxide were added slowly and mixed evenly; (3) the mixer was increased to 1000r / min and stirred for 30min; (4) Grind the fineness to below 20 μ m, reduce the speed, add the remaining raw materials, and mix evenly; (5) stop the machine, filter, discharge the materials, load the barrels, and put them into storage Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.