Key tips: 1 Construction process of imitation marble coating: Base treatment of wall surface → scraping (plastering) anti crack mortar and compounding alkali resistant glass fiber mesh cloth → scraping (plastering) 2-3 times of flexible water-resistant putty → brushing (spraying) 1 time of special sealing primer → brushing (spraying) 1-2 times of intermediate paint → snapping, dividing and pasting tape → spraying liquid granite coating material 2 times → spraying liquid granite coating and finishing paint 2-3 times 2、 Precautions for marble like coating construction: 1, Shi Paint knowledge | precautions for wall paint color selection Recommended introduction: when painting the wall, the owner sometimes has difficulty in choosing what color of the wall paint to paint In fact, there is no ugly color in the wall paint, only the disharmonious color matching The use of wall color contains the knowledge of health Too strong color will stimulate people's perception, make people have a sense of fidgety, affect people's mental health Grasp the basic principles of wall color and paint a colorful space 1、 Wall paint color selection notice 1 Light color is generally used for the top surface Light colors make people feel light, dark colors make people feel heavy Usually, the treatment of rooms is from top to bottom, from shallow to deep For example, the ceiling and walls of rooms are white and Paint Home News: 1 Construction process of imitation marble paint: wall base treatment → scraping (plastering) anti crack mortar and composite alkali resistant glass fiber mesh cloth → scraping (plastering) 2-3 times of flexible water-resistant putty → brushing (spraying) 1 time of special sealing primer → brushing (spraying) 1-2 times of intermediate paint → Snapping line, dividing grid and sticking tape → spraying liquid granite coating twice → spraying liquid granite coating twice or three times 2、 Precautions for the construction of imitation marble coating: 1 The construction temperature is above 5 ℃, and it is not suitable for construction in windy weather after rain 2 It is forbidden to mix with other coatings, and the construction effect of matching products is better 3 The next process can only be carried out after the primer is dried 4 The spraying pressure is 0.3-0.4mpa The spray gun can be a professional spray gun with a diameter of 2.5mm 5 After use, the remaining coating shall be sealed and stored in a cool place 6 The storage temperature is 5-30 ℃, and the shelf life is one year Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only.
This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of
the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed
description of the concern or complaint, to
service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content
will be removed immediately.