    Coating technology: production and preparation method of jade paint

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Core tip: preparation of jade paint additive: inject 200 parts of water into the reactor, heat up to 90 ℃ - 100 ℃, add 300-310 parts of 108 glue to dissolve, evaporate, mildew resistant, defoamer, boil and dissolve, then cool to room temperature, and obtain 320-340 parts of viscous additive for use The crude jade is ground and finely screened into 400 mesh powder The bactericide is saturated silver solution Mercury is dissolved in water in the form of steam by electrolysis to form saturated silver solution bactericide Add each component into the mixing tank, and stir it for 30min under the condition of 15 ℃ - 28 ℃ and atmospheric pressure Paint agent, top 10 Chinese wall paint brands Recommended introduction: interior wall paint and exterior wall paint can achieve beautiful, clean and pleasant effects, but the effects in different environments are different, so the color of the paint will be different There are ten brands of Chinese paint, ten brands of global paint, ten brands of Chinese wall paint, and ten brands of Chinese paint, Famous trademark of Chinese paint and coating In private rooms, most of us choose according to our own personality, personal hobbies and living habits The younger generation will choose the interior wall paint with rich colors and bright colors, while the older ones will have some working experience Coating home news: preparation of jade paint additives: inject 200 parts of water into the reactor, heat to 90 ℃ - 100 ℃, add 300-310 parts of 108 glue to dissolve, evaporate, mildew resistant, defoaming, boil to room temperature, and then get 320-340 parts of viscous additives for use The crude jade is ground and finely screened into 400 mesh powder The bactericide is saturated silver solution Mercury is dissolved in water in the form of steam by electrolysis to form saturated silver solution bactericide Add each component into the mixing tank, mix for 30min under the condition of 15 ℃ - 28 ℃ and atmospheric pressure, then the finished product will be packed and put into storage Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.