    China Paint Online News Information: Why can
    the real stone paint do a good job after not achieving their ideal results? The main reasons are two points: product and construction. So what are the problems that tend to arise in construction? The following by the Chinese

    experts for you to briefly introduce a few external wall real stone paint construction common problems and solutions.
    common problems and solutions to the construction of real stone paint on the outerFirst, uneven coloring
    the main reasons: coloring with inaccurate grasp, mixed paint can not spread evenly, the thickness of the coating caused by uneven.
    solution: re-do the secondary product uniform adjustment, until the coating on the finish has a certain texture.2, paint surface cracking and empty drum phenomenon
    the main reasons: coloring with the master is not correct, mixed paint can not be on time and evenly spread up, the thickness of the coating is not average caused.
    solution: re-do the secondary product adjustment of real stone paint, until the paint on the finish has a certain texture.3, a large number of uneven pattern phenomenon
    the main reasons: large area of cement mortar, resulting in slow drying time, which will produce cracking and empty drum phenomenon;
    solution: to carry out the average division treatment, in the base house dusting process, the mortar evenly matched.
    common problems and solutions to the construction of real stone paint on the outerFourth, the surface layer of the joint
    main reasons: excessive spraying product, resulting in the paint surface is too thick.
    solution: timely according to the scale of exchange for cement mortar surface acceptance, if not closed can not be completed as scheduled., the existence of cross-contamination serious
    the main reason: the surface layer in the construction process did not notice the distribution on the sub-section, resulting in the appearance of unrrouted.
    Solution: In the construction process must comply with every construction step to complete, try to avoid cross-contamination damage, at the same time, we can choose with anti-aging, anti-high temperature and anti-strong exposure to auxiliary coatings to fill, but also to ensure the reduction of cross-contamination.
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.