    Wood furniture is now very common furniture category, we now have a lot of people for the health of their families and environmental protection needs, in the purchase of furniture will be deliberately selected solid wood furniture, solid wood furniture in the production process there are many links and steps, one of which is painting.
    to paint furniture is a very important link, the quality of paint directly affects the degree of environmental protection and performance of furniture, painting technology also directly determines the aesthetic degree of the surface of furniture. Let's take a look at the steps for painting furniture, that is, the standard furniture painting process

    .
    furniture paint
    the paint of wooden furniture is classified according to the way, there are closed, semi-closed and open three different methods of painting, the final effect of different painting methods are also different. Specifically, the detailed texture of the wood is barely visible after the closed coating, while the open effect is more natural and shows the texture of the wood.
    the difference between the various construction methods is not large, the basic construction order: white blank plate →threding→ substrate closure (scratch putty) → grinding→ brushing primer (first time) → Grinding → brush primer (second to third times→ fully polished→ brush paint (first time) → Polishing→ brush paint (second time).
    the paint order of wood furniture
    01, sheet treatment
    before painting, first clean the wood, the wood surface dust and so on clean. Cleaning can be used with a special dust cloth, large areas such as flooring, etc. can be used vacuum cleaner repeated vacuum. At the same time with sandpaper to the board surface or wood line surface light, pay attention to protect the wood skin, can not be sand through.
    02, plate closure
    will be equipped with a good special plate closure agent, evenly painted to the plate, can effectively close the plate, to prevent contamination of the plate. Plate closure can prevent excessive moisture absorption, loose moisture and plate deformation, enhance the adhesion between the paint film and the plate, save the amount of paint, enhance the hardness of the paint film.
    03, scraping putty
    choose the matching wood putty, after the deployment, hard putty scraping to fully backlog to the wood eye. After the putty has dried, use sandpaper to polish it thoroughly and clean the putty on the wooden set. Filling wooden holes with putty can reduce the amount of wood paint and improve the flatness of the paint film. Different paint effects require different scraping requirements for putty. For example, to do an open effect, putty color should be modulation and plate color consistent before scratching.
    04, primer construction
    in accordance with the required proportion of wood primer, can be painted or sprayed and so on. The role of primer construction is to fill wood holes and increase the thickness of the paint film. When working, pay attention to the primer dry, must be thoroughly polished with sandpaper, and then apply the primer again. Requires even brushing, no flow hanging, wood-eye filling flat.
    05, sanding treatment
    sanding plate with sandpaper is actually throughout the wood paint construction process steps. Plate treatment to sand, scrape putty to sand, primer construction to sand, paint before and after construction also sanding. The steps of sanding are critical. The sanding treatment makes the sheet smoother, smoother and easier to paint. After painting sanding, and make the paint film surface flat, smooth. However, pay attention to sanding treatment to avoid cross sand, can not be used in thick sandpaper sanding.
    06, paint construction
    before the paint construction must once again clean the wood surface, remove dust particles, so that the paint film surface can have a better coating effect. Each time the paint, should not be brushed once too thick, it is best to take the method of multiple brushing, such as the paint film dry and then do the next layer of construction. Paint construction directly affects the final effect of paint film, paint construction requirements must be painted uniformly, no flow hanging, good gloss, no obvious brush marks, smooth and delicate feel.
    .
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.