echemi logo
Product
  • Product
  • Supplier
  • Inquiry
    Home > Coatings News > Paints and Coatings Market > Diatom mud technology principle and construction process

    Diatom mud technology principle and construction process

    • Last Update: 2020-12-17
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Material features
    characteristics 1: all a color earthy, high temperature coloring, a large number of spray water after no color, do not flow mud, with the palm of the palm of the light press, with the effect of natural mud.
    2: powder, stirring, construction without any odor, without any release of harmful substances.
    features 3: the texture is delicate, there are small sand particles, suitable for the smooth and dry indoor wall construction
    Chinese
    .
    characteristics 4: water absorption, fire does not ignite, does not have a pungent odor.
    Molecular sieve structure of diatom soil
    technical principles
    electron microscopes show that diatom minerals are a nanoscale porous material (micro-porous diameter of about 0.1-0.2 microns), with a porosity rate of up to 90%, and are arranged in a circular and needle-shaped arrangement, with thousands of times more fine holes per unit area than charcoal. The outstanding characteristics of molecular lattic structure determine its unique function. Diatom minerals have strong physical adsorption and ion exchange properties, after finishing is widely used in alcohol and medical injection filtration, food additives, nuclear radiation adsorbents and many other fields. Diatom precipitation forms diatom minerals - diatom soil.
    Construction process
    (1) stirring
    in the mixing container to add 90% of the water used for the construction of clean water, and then poured into the diatom mud dry powder soaked for a few minutes, and then stirred with an electric mixer for about 10 minutes, stirring while adding 10% of the water to adjust the construction viscosity, mud coating, fully stirred well before use.
    (2) smear
    twice: about 50 minutes after the first coating is about 1 mm complete (depending on the climate on site, the surface is not sticky hand, there is dewy conditions with material to level), apply the second time (thickness of about 1.5 mm).
    thickness between 1.5 mm and 3.0 mm.
    (3) texture pattern production
    smear the second time completed, according to the actual environment drying situation, master the drying time, according to the work method to make texture pattern
    (4) lighting

    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.