echemi logo
Product
  • Product
  • Supplier
  • Inquiry
    Home > Coatings News > Paints and Coatings Market > Paint formula: vinyl acetate emulsion paint formula and production process

    Paint formula: vinyl acetate emulsion paint formula and production process

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Core tip: polyvinyl acetate emulsion interior wall coating is a large class, mainly refers to vinyl acetate homopolymer and its copolymer as the base material The formulation of vinyl acetate latex paint is as follows: raw material /kg water 233 titanium dioxide 260 talcum powder 400 mesh 82 carboxymethyl cellulose 1 polymethacrylate sodium 0.8 six sodium meta phosphate, 1.5 polyvinyl acetate emulsion (40%) 422 sodium nitrite 3 3 phenyl acetate mercury total 3 Paint agent, top 10 Chinese wall paint brands Recommended introduction: interior wall paint and exterior wall paint can achieve beautiful, clean and pleasant effects, but the effects in different environments are different, so the color of the paint will be different There are ten brands of Chinese paint, ten brands of global paint, ten brands of Chinese wall paint, and ten brands of Chinese paint, Famous trademark of Chinese paint and coating In private rooms, most of us choose according to our own personality, personal hobbies and living habits The younger generation will choose the interior wall paint with rich colors and bright colors, while the older ones will have some working experience Coatings home: polyvinyl acetate emulsion interior wall coating is a large class, mainly refers to vinyl acetate homopolymer and its copolymer as the base material The formulation of vinyl acetate latex paint is as follows: raw materials for coating materials /kg water 233 titanium dioxide 260 talcum powder 400 mesh 82 carboxymethyl cellulose 1 polymethacrylate sodium 0.8 six sodium meta phosphate, 1.5 polyvinyl acetate emulsion (40%) 422 sodium nitrite 3 3 phenyl mercuric chloride The water, titanium dioxide, talcum powder, carboxymethyl cellulose, sodium methacrylate and six sodium hypophosphite were added to the high-speed dispersing machine After mixing evenly, the 20-30min was dispersed at high speed The polyvinyl acetate emulsion, sodium nitrite and phenyl mercuric acetate were stirred evenly under low speed, and then filtered, packed and stored Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.