    In the spraying operation, the paint film drying did not cure in the specified time, hand touch paint film has the feeling of wet re-moisture, resulting in the overall hardness of the paint film is low.
    not reach the required hardness or there is a dry phenomenon in the watch, polishing there are prints, wipe with a towel there are traces.
    hardness - cause:
    1, did not choose the appropriate curing agent and thinner by temperature

    .
    2, added a poor quality thinner.
    3, improper ratio of deployment, coating is too thick.
    4, rough grinding.
    5, did not do closed primer,
    cylinder
    substrate absorbs a large number of solvents.
    hardness - prevention:
    1, according to the temperature of the correct choice of the right curing agent and thinner.
    2, the substrate needs to be thoroughly dried and polished.
    3, color paint layer should not be sprayed too thick.
    4, the use of 2K primer for closed isolation treatment.
    5, all 2K series paint, after deployment, static storage for about 5 minutes before construction.
    hardness - solution:
    the coating is thoroughly polished and re-sprayed correctly.
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.