    What is the reason why the results of the salt spray test of electrophoresis paint film are not qualified?

    • Last Update: 2020-12-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Electrophoresis coating has been widely used in automobiles, motorcycles, bicycles, home appliances because of its safety and environmental protection, excellent quality control, high efficiency of operation and production... and so on all walks of life. The most basic purpose of coating is anti-corrosion, but sometimes it is also found that the finished electrophoresis of the salt spray test results are not ideal, why? Explain the reasons and prevention methods for everyone now.
    common causes of poor salt spray testing in finished electrophoresis products: poor pre-treatment of
    (
    1
    ), corrosion of work parts before electrophoresis has produced .
    (
    2
    ) electrophoretic tank liquid too many impurity ions, deposition mixed into the electrophoretic paint film.
    (
    3
    ) electrophoresis paint film thickness is thin.
    (
    4
    ) after electrophoresis water washing salt more.
    (
    5
    ) electrophoresis paint film is not cured completely.
    control methods:
    (
    1
    ) strictly in accordance with the requirements of pre-treatment control, to ensure the quality of phosphate film.
    (
    2
    ) reduces the concentration of impurity ions in the electrophoresis tank by controlling the conductivity of the fluid in the tank.
    (
    3
    ) strictly in accordance with the requirements of the process, to ensure that the thickness of electrophoresis paint film up to the target requirements.
    (
    4
    ) is rinsed with pure water, and the conductivity of the water is controlled
    below 50um/cm
    cm.
    (
    5
    ) classify electrical swimming for work items of different thicknesses, strictly control baking time and temperature, and ensure that the coating film is fully cured.
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.