Formula of epoxy anticorrosive paint with non-toxic paint film and non-pollution to water
Time of Update: 2021-03-17
Then add an appropriate amount of toughening agent to the resin system obtained in step 1, and disperse at a high speed to uniformly disperse various substances.
Add various additives to the base material of step 2, and disperse at high speed.
-
Proportion and preparation method of dry powder latex paint for interior wall
Time of Update: 2021-03-17
Therefore, the dry powder latex paint for interior walls per unit mass has a large construction area with a theoretical value of 25~35m2/(kg·layer), which is suitable for Surface finishing of indoor plaster walls, concrete, masonry buildings, gypsum, brick walls, wooden boards, asbestos boards, etc.
-
Interior wall latex paint formula four
Time of Update: 2021-03-17
Formulation characteristicsThe multi-element titanium dioxide additive AY-726W used in this product has high hiding power, low oil absorption, and good chemical stability, which greatly improves the p
-
Nano negative ion antibacterial environmental protection latex paint formula
Time of Update: 2021-03-17
Under low-speed stirring less than 500r/min, first add dispersant, wetting agent, pH adjuster, and part of defoaming agent to deionized water according to the formula (parts by mass), fully disperse uniformly, and then add Fillers, pigments and functional materials are dispersed at a high speed for more than 50 minutes at a speed greater than 1200r/min, and the detection fineness is ≤50μm, and then add water-based emulsion, film-forming additives, and residual waste at a medium speed of 400~800r/min.
-
How much do you know about elastic latex paint?
Time of Update: 2021-03-17
5~2, 215 titanium dioxide 45~55, wollastonite powder 80~150, kaolin 40~60, 800 mesh heavy calcium carbonate 120~180 , Water-based fluorocarbon resin 100~120, styrene-acrylic emulsion 50~100, elastic emulsion 250~300, film forming aid 5~20, wetting agent X-405 1~3, rheology modifier 2~5, increasing Thickener 5~10.
-
Water-based reflective thermal insulation coating formulation
Time of Update: 2021-03-17
Under the condition of stirring and dispersing at a low speed of 500r/min, add emulsion, hollow glass beads, film forming aids, Hydropalat-306, propylene glycol and FoamStar A-34 defoamer to the pigment and filler slurry.
-
The characteristics and classification of rosin-modified phenolic resin and its application in offset printing inks
Time of Update: 2021-03-17
Due to the unique honeycomb structure characteristics of rosin-modified phenolic resin, it has a good wetting effect on the pigments, and a certain viscoelastic binder can be obtained after proper reaction with the gelling agent, so it is widely used in offset printing inks.
-
Modern water-based coating technology, formulation and application
Time of Update: 2021-03-17
The third chapter discusses the application of water-based coatings in the field of construction and industrial coating extensively on the basis of systematic discussion of water-based coating production technology, production technology and formula, and finally briefly introduces the quality assurance system of water-based coatings.
-
Download the 2015 edition of alkyd resin coatings for free
Time of Update: 2021-03-17
Chapters 1 to 5 are introduction, manufacturing principles, technology, development status, and production process pollution prevention of alkyd resin coatings, driers, etc.
The sol-gel technology modification and the synthesis and performance of hyperbranched alkyd (polyester) resin are listed in a separate chapter, in order to attract readers' attention.
-
Building interior latex paint formula
Time of Update: 2021-03-17
Formulation characteristicsThis product does not contain mercury and its compounds, and does not use lead, cadmium, chromium and its compound pigments to reduce or reduce the content of toxic and harmful volatile organic compounds and heavy metal ions as much as possible to ensure that the coating has better physical properties.
-
Environment-friendly thermal insulation nano coating formula
Time of Update: 2021-03-17
PrecautionsThe range of the mass ratio of each component of the environmentally friendly thermal insulation nano coating formulation is: synthetic water-based resin 140~750, nano-pigment and filler slurry 50~100, film forming aid 10~20, coupling agent 5~20, defoaming Agent 5-10, leveling agent 5-10, wetting agent 5-10.
-
Fluorosilicon modified acrylic resin hydrophobic anticorrosive coating formulation
Time of Update: 2021-03-17
B-component preparation method: package the curing agent separately.
-
What are the differences between metallic paint and ordinary paint?
Time of Update: 2021-03-17
The most typical colors of ordinary paint are black, red and white.
The most typical colors of ordinary paint are gray-black, bright red and milky white.
2. The difference between lacquerCompared with ordinary paint, the paint surface of metal paint is harder.
-
Free download of powder coating and raw material inspection method manual
Time of Update: 2021-03-17
brief introductionThis book introduces in detail the inspection methods of powder coatings, epoxy resins, polyester resins, acrylic resins, powder coating additives, pigments and fillers.
Chapter Four Performance Inspection of Acrylic Resin and Its Curing Agent
-
Blue interior wall latex paint formula check
Time of Update: 2021-03-17
After the filtration is completed, under low-speed stirring, add wetting agent, defoamer, film-forming aid, emulsion to the above-mentioned dispersion slurry, and then add thickener to adjust the viscosity to 90~100KU, add pH adjuster to make the pH Value is 8.
-
Check the formula of internal and external wall latex paint
Time of Update: 2021-03-17
1. In addition to conventional emulsions, pigments, fillers, and additives, the latex paint for interior and exterior walls of this product also contains isolated whey protein extracted from milk as a film-forming substance.
-
Formula of water-based stain-resistant heat-reflective phase change thermal insulation coating
Time of Update: 2021-03-17
PrecautionsThe mass ratio of each component of the water-borne stain-resistant heat-reflective phase-change heat-insulating coating formula is as follows: film-forming emulsion 25-50, heat-reflective pigment 10-25, infrared emission filler 2-15, additive 1-6, and Ionized water 20~30.
-
Check the formula of high solids water-based interior wall latex paint
Time of Update: 2021-03-17
Recipe details (parts by mass)Production MethodDuring the preparation, the pigment and filler dispersion stage: add water, cosolvent, wetting agent, dispersant, defoamer, pigment and filler in sequence, and disperse at high speed until the pigment and filler reach the specified fineness.
Paint mixing stage: Add emulsion, film-forming aids, and thickeners in sequence under low-speed stirring to make qualified finished products.
-
Correlation between xenon lamp aging and pigment weather resistance from natural exposure testing (2)
Time of Update: 2021-03-16
the data in Figures 4 and 5, it can be seen that the color of each sample changes, whether it is outdoor exposure or xenon lamp acceleration testing, and the value of DE increases as the test time increases.
-
Application of redstone nano-titanium dioxide in vehicle coatings (2)
Time of Update: 2021-03-15
From Table 3, it can be seen that NTG-602nm titanium dioxide is of great help to improve the weather resistance of light blue acrylic metal drying paint, with the increase of NTG-602B nano-titanium dioxide addition, the coating film after artificial aging to produce loss of light, color change phenomenon decreasing, because nano-titanium dioxide has the effect of ultraviolet absorption, scattering function.