    Home > Coatings News > Paints and Coatings Market > Coating process: formulation and process of non toxic antifouling coating of zinc acrylate resin

    Coating process: formulation and process of non toxic antifouling coating of zinc acrylate resin

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Core tips: the basic formula of zinc acrylate non-toxic antifouling coating: Nominal quality /% Tallow 20-25 Silicate 10-40 Zinc oxide 5-15 Dispersant 0.5 ~ 1 Antifouling agent 1 5 ~ 10 Antifouling agent 2 1 ~ 2 Anti settling agent 0.1 ~ 0.5 Solubilizer 10~ Paint knowledge how about Akzo Nobel Powder Coating Recommended introduction: powder coating is a kind of coating with different form from general coating, which is in powder form It is a new type of coating, because of its own advantages and more and more known by people Let's introduce Akzo Nobel Powder coating Akzo Nobel Powder coating is a cost-effective coating solution, which can be applied to different kinds of products After the treatment of static electricity and fire baking, a tough and durable coating surface will be formed, with the least impact on the environment Since the introduction of this technology, powder coating has been able to continue to maintain the Home of coatings: the basic formula of non-toxic antifouling coating of acrylic zinc resin: nominal weight /% resin 20 ~ 25 silicate 10 ~ 40 zinc oxide 5 ~ 15 dispersant 0.5 ~ 1 antifouling agent 15 ~ 10 antifouling agent 21 ~ 2 anti settling agent 0.1 ~ 0.5 dissolving agent 10 ~ 20 ① check the equipment carefully before production to make it in a clean and intact state, and operators shall wear safety protection products ② The resin, antifouling agent (such as cuprous oxide), pigments and fillers (such as titanium dioxide, iron oxide red, zinc oxide, etc.) and solvent (such as xylene, ethyl acetate, etc.) are respectively weighed according to the design formula and added to the batching tank After adding the materials, the high-speed mixer shall be used to stir them for more than 30min ③ The prepared materials are ground by ball milling, and the grinding time is more than 1h The fineness of coating is measured by scraper fineness meter Generally, when the fineness of the coating reaches below 50 mesh, it can meet the requirements, and then filter and repack the coating for later use ④ Clean the equipment and production site in time after production Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.