    Core tips: 1, acrylic latex repair primer formula: paint formulation dosage /kg water 159.32 hydroxyethyl cellulose 1.67 ammonia 0.84 dispersant 13.01 wetting agent 2.04 titanium white 139.43 calcium carbonate 102.25 barium phosphate 92.95 acrylic emulsion 556.14 alcohol ester twelve twelve ethylene glycol sodium nitrite aqueous solution defoaming agent, acrylic latex repair primer production process: (1) Prepare raw materials according to the paint formula; (2) Add water to the paint dispersion mixer Paint agent, top 10 Chinese wall paint brands Recommended introduction: interior wall paint and exterior wall paint can achieve beautiful, clean and pleasant effects, but the effects in different environments are different, so the color of the paint will be different There are ten brands of Chinese paint, ten brands of global paint, ten brands of Chinese wall paint, and ten brands of Chinese paint, Famous trademark of Chinese paint and coating In private rooms, most of us choose according to our own personality, personal hobbies and living habits The younger generation will choose the interior wall paint with rich colors and bright colors, while the older ones will have some working experience Coatings home news: 1, acrylic latex repair primer formula: coating formulation dosage /kg water 159.32 hydroxyethyl cellulose 1.67 ammonia 0.84 dispersant 13.01 wetting agent 2.04 titanium white 139.43 calcium carbonate 102.25 barium phosphate 92.95 acrylic emulsion 556.14 alcohol ester twelve twelve ethylene glycol sodium nitrite aqueous solution defoaming agent, acrylic latex repair primer production process: (1) Prepare the raw materials according to the paint formula; (2) add the water into the pull cylinder of the paint dispersion mixer, start the mixer (rotating speed: 300r / min), and slowly add hydroxyethyl cellulose, ammonia, glycol, dispersant, surfactant, titanium dioxide, calcium carbonate and barium metaphosphate in turn and mix them evenly; (3) increase the mixer rotating speed to more than 1000r / min and mix for 20-30 minutes; (4) After the test fineness is qualified, reduce the speed, add the remaining components, adjust the pH value to 9.3 ~ 9.5, and mix evenly; (5) shut down, filter, discharge, barrel and put into storage Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Related Articles

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.