    Core tips: 1, alkyd modified polyvinyl acetate latex paint formulations: raw material dosage of /KG water 375.7 bactericides 5KTPP1.5 lecithin 6 defoamer 1 ethylene glycol 18.6 titanium white 250 magnesium silicate 125 Hydroxyethyl Cellulose 3 alcohol ester twelve 12 surface agent 2 emulsion approximation alkyd resin, alkyd modified polyvinyl acetate latex paint production process: (1) Prepare raw materials according to the paint formula; (2) Add 167kg water into the pull cylinder of the paint dispersion mixer, start the mixer (rotating speed: 300r / min), and slowly add the bactericide and KT in turn Paint agent, top 10 Chinese wall paint brands Recommended introduction: interior wall paint and exterior wall paint can achieve beautiful, clean and pleasant effects, but the effects in different environments are different, so the color of the paint will be different There are ten brands of Chinese paint, ten brands of global paint, ten brands of Chinese wall paint, and ten brands of Chinese paint, Famous trademark of Chinese paint and coating In private rooms, most of us choose according to our own personality, personal hobbies and living habits The younger generation will choose the interior wall paint with rich colors and bright colors, while the older ones will have some working experience Coatings home news: 1, alkyd modified polyvinyl acetate latex paint formulations: raw material consumption of /KG water 375.7 bactericides 5KTPP1.5 lecithin 6 defoamer 1 ethylene glycol 18.6 titanium white 250 magnesium silicate 125 Hydroxyethyl Cellulose 3 alcohol ester twelve 12 surface agent 2 emulsion approximation alkyd resin, alkyd modified polyvinyl acetate latex paint production process: (Wei) according to the paint formula to prepare raw materials; (2) 167kg water is added into the pull cylinder of the paint dispersion mixer, the mixer is started (rotating speed is 300r / min), and then the bactericide, ktpp, lecithin, 1kg defoamer, glycol, titanium dioxide and magnesium silicate are added slowly and mixed evenly; (3) the mixer is adjusted to above 1000r / min and stirred for 20 minutes; (4) After the test fineness is qualified, reduce the speed, add the remaining components, adjust the pH to 8.8, and mix evenly; (5) stop the machine, filter, discharge, barrel and store in the warehouse Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Related Articles

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.