    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Core tips: 1, ethylene propylene glossy latex paint formulations: raw materials for coating /kg water 35 thickeners, 5 ammonia (28%), 6 dispersant 2, sodium hypophosphite, 15, film additives, 57.4 defoamer, 2 titanium white R820158.3, ethylene propylene emulsion (42%), homemade) mixture of 42% mixture (homemade), anti mildew mixture, mixture of name, dosage, /kg, pentachlorophenol sodium, sodium benzoate, sodium nitrite, water, and ethylene acrylate glossy latex paint Production process: (1) Prepare raw materials according to the paint formula; (2) Prepare the mixture: add 130.4kg water Shenyang steel structure fireproof coating construction expert punde Building Fire Engineering Co., Ltd Recommended introduction: since its establishment, Shenyang punde Construction Fire Engineering Co., Ltd has cultivated a group of professional construction teams with excellent equipment, rich experience and serious responsibility with advanced and scientific management methods and strict engineering quality assurance and after-sales service system It has undertaken a number of fire system installation projects, which has been praised by customers Every idea and special requirement of you will be fully considered by us and fully realized in the construction technology, which will become the cornerstone of our successful long-term development We are looking forward to your invitation, to provide you with quality services and high-quality technical support! All construction coatings have passed ISO9001 Coatings home news: 1, ethylene propylene glossy latex paint formulations: raw materials for coating materials, /kg water 35 thickeners, 5 ammonia (28%) 6 dispersant 2 six sodium diphosphate, 15 film forming AIDS, 57.4 defoamer 2 titanium white R820158.3 ethylene propylene emulsion (42%, homemade) 42% mixture (homemade), anti mildew agent, mixed liquid: Component name and dosage / kg sodium pentachlorophenol 4.8 sodium benzoate 8 sodium nitrite 0.8 water 130.42, production process of ethylene propylene light emulsion paint: (1) prepare raw materials according to the paint formula; (2) prepare the mixture: add 130.4kg water into the plastic bucket, slowly add sodium pentachlorophenol, sodium benzoate and sodium nitrite while stirring, fully mix and mix evenly, and reserve (3) Add the water into the drawing cylinder of the paint dispersion mixer, start the mixer (rotating speed: 300r / min), slowly add thickener, ammonia water, dispersant, sodium hexametaphosphate, film forming assistant, 1kg defoamer and titanium dioxide to mix evenly; (4) increase the mixer rotating speed to more than 1000r / min and mix for 20 minutes; (5) Test the fineness to below 30 μ m, reduce the speed, add 14.4kg of the remaining components and self-made mixture, and mix evenly; (6) stop the machine, discharge the material, load the barrel, and put it into storage Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.