echemi logo
Product
  • Product
  • Supplier
  • Inquiry
    Home > Coatings News > Paints and Coatings Market > Coating process: production process of high concentration emulsion paint for interior wall

    Coating process: production process of high concentration emulsion paint for interior wall

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Core tips: 1 High concentrated latex paint formula for interior wall: quality of coating raw materials, /kg water 150 glycol 20 dispersant 5 defoamer 2.5 wetting agent preservative 1 anatase titanium white 120 120 lithopone 60 heavy calcium 200 kaolin 50 talc powder 80 film builder, 80 styrene acrylic emulsion, thickener, ammonia water and high concentrated latex paint (1) Prepare the raw materials according to the emulsion paint formula; (2) Water, glycol, dispersant, 5kg defoamer, preservative, titanium dioxide, wetting agent, bicalcium, talcum powder, kaolin and lithopone shall be treated in accordance with the requirements Paint knowledge how about Akzo Nobel Powder Coating Recommended introduction: powder coating is a kind of coating with different form from general coating, which is in powder form It is a new type of coating, because of its own advantages and more and more known by people Let's introduce Akzo Nobel Powder coating Akzo Nobel Powder coating is a cost-effective coating solution, which can be applied to different kinds of products After the treatment of static electricity and fire baking, a tough and durable coating surface will be formed, with the least impact on the environment Since the introduction of this technology, powder coating has been able to continue to maintain the Paint Home News: 1, interior wall high concentrated latex paint formula: paint raw material quality /kg water 150 ethylene glycol 20 dispersant 5 defoamer 2.5 wetting agent preservative 1 anatase titanium white 120 lithopone 60 heavy calcium 200 kaolin 50 talc powder 80 film builder 80 styrene acrylic emulsion thickening agent ammonia ammonia water, interior wall high concentration latex paint production process: (d) according to the above latex paint formula to prepare raw materials; (2) Add water, glycol, dispersant, 5kg defoamer, preservative, titanium dioxide, wetting agent, heavy calcium, talcum powder, kaolin and lithopone into the paint mixing barrel in sequence, start the mixer to mix (high-speed dispersion, 1000r / min) until the fineness is less than 30 μ m; (3) add the remaining components in the latex paint formula in a further step, and mix evenly; (4) Use chemical pump to input the mixed emulsion paint into the grinder, grind to the required fineness, discharge, filter, barrel and storage Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.