Coating process: production process of polyvinyl alcohol bentonite interior wall coating
-
Last Update: 2020-04-03
-
Source: Internet
-
Author: User
Search more information of high quality chemicals, good prices and reliable suppliers, visit
www.echemi.com
Core tips: 1 Formulation of PVA bentonite interior wall coating: raw material consumption / kg PVA 16 bentonite (calcium or sodium 320 mesh) 20 attapulgite (320 mesh) 20 talcum powder (320 mesh) 80 light calcium carbonate (320 mesh) 160 wollastonite powder (320 mesh) 20 water-soluble coating paste appropriate other additives 6 water 5002 Production process of PVA bentonite interior wall coating: (1) Prepare raw materials according to the paint formula; (2) Add polyvinyl alcohol into the drawing cylinder of the paint dispersion mixer, and start the mixer (rotating speed: 300r / min) Which is the price of Dajin diatom mud Recommended brief introduction: which is the price of Dajin diatom mud? How to buy genuine diatom mud? Guangdong diatom mud agent suggests placing a basin of cold water in the air conditioning room, so that the diatom mud wall can breathe effectively The feature of the breathing wall is obvious When the indoor air is dry, the diatom mud wall will release the absorbed water quickly Put it out to help regulate the indoor dry humidity It is suggested to place a basin of cold water in the air conditioning room, so that the wall of diatom mud can breathe effectively The feature of the wall that can breathe is obvious When the indoor air is relatively dry, the wall of diatom mud will absorb the water Home of coatings: 1 Formulation of polyvinyl alcohol bentonite interior wall coating: raw material consumption / kg polyvinyl alcohol 16 bentonite (calcium or sodium 320 mesh) 20 attapulgite (320 mesh) 20 talcum powder (320 mesh) 80 light calcium carbonate (320 mesh) 160 wollastonite powder (320 mesh) 20 water soluble coating material color paste appropriate amount of other additives 6 water 5002 Production process of polyvinyl alcohol bentonite interior wall coating: (1) Prepare the raw materials according to the paint formula; (2) add polyvinyl alcohol into the pull cylinder of the paint dispersion mixer, start the mixer (rotating speed: 300r / min), and then slowly add bentonite, attapulgite, talcum powder, light calcium carbonate and wollastonite powder to mix evenly; (3) increase the mixer rotating speed to more than 1000r / min, and mix for 20 minutes; (4) Test the fineness, reduce the speed after passing the test, add the remaining components, and mix evenly; (5) stop the machine, filter, discharge, barrel and store in the warehouse Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only.
This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of
the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed
description of the concern or complaint, to
service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content
will be removed immediately.