    Coating process: production process of real stone paint

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Core tip: production process of real stone paint (take 1t as an example) 1 Add 100kg water into the dispersion tank and rotate it at medium speed (500-600 R / min); 2 Slowly add 1.5 kg of hydroxyethyl cellulose into the dispersion tank, and disperse at high speed (1000-1200 R / min) for 20-30 minutes until all the hydroxyethyl cellulose is dissolved; 3 Add 1.5kg ammonia water and 9kg film forming agent, and mix evenly; 4 Add 150 emulsion and 1.5 defoamer to mix evenly 5 Pump the above evenly stirred slurry into the special equipment for real stone paint Which is the price of Dajin diatom mud Recommended brief introduction: which is the price of Dajin diatom mud? How to buy genuine diatom mud? Guangdong diatom mud agent suggests placing a basin of cold water in the air conditioning room, so that the diatom mud wall can breathe effectively The feature of the breathing wall is obvious When the indoor air is dry, the diatom mud wall will release the absorbed water quickly Put it out to help regulate the indoor dry humidity It is suggested to place a basin of cold water in the air conditioning room, so that the wall of diatom mud can breathe effectively The feature of the wall that can breathe is obvious When the indoor air is relatively dry, the wall of diatom mud will absorb the water Home of coatings: the production process of real stone paint (take 1 ton as an example) 1 Add 100kg water into the dispersion tank and rotate it at a medium speed (500-600 R / min); 2 Slowly add 1.5kg hydroxyethyl cellulose into the dispersion tank and disperse it at a high speed (1000-1200 R / min) for 20-30 minutes until the hydroxyethyl cellulose is completely dissolved; 3 Add 1.5kg ammonia water and 9kg film forming assistant and mix evenly; 4, add 150 emulsion and 1.5 defoamer to mix evenly; 5, mix the above evenly stirred slurry into the special equipment for the real stone paint; 6, in the mixing state, add 740 color sand into the special equipment for the genuine stone paint, stir for about 30 minutes to even; 7, detect the material and barrel Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.