    Coating process: production process of vinyl acetate vinyl copolymer emulsion paint

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Core tips: 1, vinyl acetate ethylene copolymer latex paint formulations: raw materials, /KG water 164 dispersant 10 wetting agent 3 defoamer 4 titanium white 250 calcium carbonate 175 flame retardant 50 thickener 2 vinyl acetate ethylene emulsion 343 hydroxyethyl cellulose 174 propylene glycol alcohol ester ester 174, vinyl acetate ethylene copolymer latex paint production process: (1) Prepare raw materials according to the paint formula; (2) Add 125kg water into the pull cylinder of the paint dispersion mixer, start the mixer (rotating speed: 300r / min), and slowly add dispersant, wetting agent and defoaming agent in turn Application scope and advantages of roller ceramic coating Recommended introduction: the surface of ceramic rubber plate used for roller ceramic coating is cast into durable rubber plate by hundreds of independent small ceramic pieces Each ceramic piece has raised characteristics Under general conveyor belt pressure, thousands of unique cast bumps can produce positive traction, prevent slipping and extend the service life of conveyor belt roller At the same time, the bottom layer adopts high-quality rubber, which has strong elasticity and can play a good impact resistance role The scope of application of roller ceramic coating is one three six 83857180 (the same as V) 1 Roller coating in extremely harsh working environment 2 The belt joint is not suitable for fixing with iron buckle; 3 It is suitable for leather Coatings home news: 1, vinyl acetate ethylene copolymer latex paint formula: raw material dosage of /KG water 164 dispersant 10 wetting agent 3 defoaming agent 4 titanium white powder 250 calcium carbonate 175 flame retardant 50 thickener 2 vinyl acetate ethylene emulsion 343 hydroxyethyl cellulose 174 propylene glycol alcohol ester ester 174, acetic acid ethylene vinyl copolymer latex paint production process: (d) according to the paint formula quantity of raw materials; (2) 125kg water is added into the pull cylinder of the paint dispersion mixer, the mixer is started (rotating speed is 300r / min), the dispersant, wetting agent, defoamer 2kg, titanium dioxide, calcium carbonate, flame retardant and thickener are added slowly in turn, and the mixture is even; (3) the mixer rotating speed is increased to more than 1000r / min, and the mixture is stirred for 20 minutes; (4) Test the fineness, reduce the speed after passing the test, add the remaining components, and mix evenly; (5) stop the machine, filter, discharge, barrel and store in the warehouse Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.