    The key points are as follows: (1) prepare raw materials according to the coating formula; (2) Add 111kg water into the pull cylinder of the paint dispersion mixer, start the mixer (rotating speed: 300r / min), slowly add ammonia water, thermosetting acrylic resin, defoamer and rutile titanium dioxide in turn, and mix evenly; (3) Raise the speed of mixer to above 1000r / min, and mix for 20-30min; (4) Reduce the speed, add the remaining raw materials, adjust the viscosity to be qualified, and mix evenly; (5) Shut down, filter Shenyang steel structure fireproof coating construction expert punde Building Fire Engineering Co., Ltd Recommended introduction: since its establishment, Shenyang punde Construction Fire Engineering Co., Ltd has cultivated a group of professional construction teams with excellent equipment, rich experience and serious responsibility with advanced and scientific management methods and strict engineering quality assurance and after-sales service system It has undertaken a number of fire system installation projects, which has been praised by customers Every idea and special requirement of you will be fully considered by us and fully realized in the construction technology, which will become the cornerstone of our successful long-term development We are looking forward to your invitation, to provide you with quality services and high-quality technical support! All construction coatings have passed ISO9001 Paint Home News: (1) prepare raw materials according to the paint formula; (2) add 111kg of water into the pull cylinder of the paint dispersion mixer, start the mixer (rotating speed: 300r / min), slowly add ammonia water, thermosetting acrylic resin, defoamer, rutile titanium dioxide and mix them evenly; (3) increase the mixer rotating speed to more than 1000r / min and mix for 20-30min; (4) Reduce the speed, add the remaining raw materials, adjust the viscosity to be qualified, and mix evenly; (5) stop the machine, filter, discharge the materials, load the barrels, and store them in the warehouse Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Related Articles

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.