Categories
-
Pharmaceutical Intermediates
-
Active Pharmaceutical Ingredients
-
Food Additives
- Industrial Coatings
- Agrochemicals
- Dyes and Pigments
- Surfactant
- Flavors and Fragrances
- Chemical Reagents
- Catalyst and Auxiliary
- Natural Products
- Inorganic Chemistry
-
Organic Chemistry
-
Biochemical Engineering
- Analytical Chemistry
- Cosmetic Ingredient
-
Pharmaceutical Intermediates
Promotion
ECHEMI Mall
Wholesale
Weekly Price
Exhibition
News
-
Trade Service
Home decoration, paint painting can be said to be a beautifying decoration project, although seemingly simple but also a technical work, so if there are defects, the overall aesthetic impact on the house is great. Of course, can put an end to this situation in advance is naturally the best, but if there has been a problem, do not have to worry, small editor this to introduce you to paint brushing problem solutions.
1 paint film whitening
nitro varnish if it is painted on rainy days or wet season, prone to whitening phenomenon, the coating will be white after the formation of an opaque or translucent milky white fog layer, colored paint white after the loss of bright colors
C.
. Therefore, attention should be paid to the construction of indoor dry, rainy days should close the window construction, if the temperature can not be controlled, you can add appropriate moisture in the paint.
2 color flower
If the color paint is two or more colors of the paint blend, the paint film may appear uneven color situation, so before painting should be mixed with a wooden stick paint, brushing if you find that the color is not uniform, you can first brush some uniform paint to uneven places, while brushing, if necessary, can be appropriate to brush several times.
3
After brushing the first paint, if the paint film is too smooth, or there is water dust on it, it will make the brush behind can not stick in the corresponding place, and the formation of speckle phenomenon, so after waiting for the first paint dry, should first wipe off the surface attached to the oil, etc., and then brush the second time.
4
because of the latex paint construction temperature is low, failed to form a continuous coating film and cracking, water will fall off;
5' wrinkled
wrinkle will make the paint film appear a lot of twists and turns or high and low uneven situation, mainly because the paint film internal dry caused, or because the coating is too thick, paint film viscosity is too large and other reasons, so should choose a moderate viscosity paint, and pay attention to the paint film should not be too thick, to avoid direct sunlight and strong winds.
6 s surface particles
surface particles are caused by the grass-roots clean-up is not completely dust residue caused, if there is dust or construction is not clean, let the dust fall on the paint surface has not solidified, so it will form particles, so in the construction should ensure that the room clean and dust-free, paint buckets, brushes to ensure clean, if the surface of particles, you can use sand paper polishing and then brush again.
paint in the process of painting may appear a variety of problems, these are to distinguish between solutions, the above just introduced to you several common problems and solutions, I hope to help you.