    Core tips: 1 Self drying or baking red enamel formula: paint raw material amount / kg water 124 ammonia 8.5 thermosetting acrylic resin 60 defoamer 5 Molybdate Orange 125 glycol butyl ether acetate 90.5 acrylic resin 5872, main performance: nonvolatile /% (mass) 39.9 color base ratio 1.0 / 2.19ph7.7 ~ 8.0 construction method spraying viscosity / Ku80 ~ 90 curing air drying or baking (paint formula in this paper is only for reference) Paint knowledge | precautions for wall paint color selection Recommended introduction: when painting the wall, the owner sometimes has difficulty in choosing what color of the wall paint to paint In fact, there is no ugly color in the wall paint, only the disharmonious color matching The use of wall color contains the knowledge of health Too strong color will stimulate people's perception, make people have a sense of fidgety, affect people's mental health Grasp the basic principles of wall color and paint a colorful space 1、 Wall paint color selection notice 1 Light color is generally used for the top surface Light colors make people feel light, dark colors make people feel heavy Usually, the treatment of rooms is from top to bottom, from shallow to deep For example, the ceiling and walls of rooms are white and Paint Home News: 1 Self drying or baking red enamel formula: paint raw material consumption / kg water 124 ammonia 8.5 thermosetting acrylic resin 60 defoamer 5 Molybdate Orange 125 glycol butyl ether acetate 90.5 acrylic resin 587 2 Main performance: non volatile matter /% (mass) 39.9 color base ratio 1.0 / 2.19ph7.7 ~ 8.0 construction method spraying viscosity / Ku80 ~ 90 curing gas drying or baking (the paint formula in this paper is for reference only) paint home is focused on the news and information of coating, diatom mud, paint coating, coating process, fire retardant coating, and coating, diatom mud, paint coating, coating process, decoration knowledge and decoration effect map of fire retardant coating,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.