    Paint knowledge | main defects of latex paint coating: blooming

    • Last Update: 2020-04-03
    • Source: Internet
    • Author: User
    Search more information of high quality chemicals, good prices and reliable suppliers, visit www.echemi.com
    Core tips: reasons: · too large dilution ratio; · smooth and dense base material does not absorb; · coating film thickness is too thin; dark paint film thickness is not enough, coating times are too few; · product covering power is not good ·The poor flatness of the base material results in uneven glossy reflection of the glossy products, which leads to blooming Prevention methods: · keep a certain roughness of the base material, and the base material of the glossy product should have a good flatness; · strictly control the dilution ratio; · control the film thickness and the number of coating layers according to the product requirements; properly increase the number of coating layers of the dark paint, and directly coating without dilution; · select high-quality paint Which is the price of Dajin diatom mud Recommended brief introduction: which is the price of Dajin diatom mud? How to buy genuine diatom mud? Guangdong diatom mud agent suggests placing a basin of cold water in the air conditioning room, so that the diatom mud wall can breathe effectively The feature of the breathing wall is obvious When the indoor air is dry, the diatom mud wall will release the absorbed water quickly Put it out to help regulate the indoor dry humidity It is suggested to place a basin of cold water in the air conditioning room, so that the wall of diatom mud can breathe effectively The feature of the wall that can breathe is obvious When the indoor air is relatively dry, the wall of diatom mud will absorb the water Paint Home News: reasons: · dilution ratio is too large; · the base material is smooth and dense without absorption; · coating film thickness is too thin; dark paint film thickness is not enough, coating times are too few; · product covering power is not good ·The poor flatness of the base material results in uneven glossy reflection of the glossy products, which leads to blooming Prevention methods: · keep a certain roughness of the substrate, and the substrate of the glossy product should have a good flatness; · strictly control the dilution ratio; · control the film thickness and the number of coating layers according to the product requirements · increase the number of coating layers of the dark paint appropriately, and directly coating without dilution; · select high-quality paint; · pay special attention to the uniform coating of the glossy product Treatment method: · after even grinding, select high-quality paint to be repainted strictly according to the process, dark paint to be repainted directly without diluent; · after the base material is treated flat, repaint Home of coatings is specialized in coatings, diatom mud, paint coating, coating technology, fire retardant coating news and coating, diatom mud, paint coating, coating technology, fire retardant coating decoration knowledge and decoration renderings,
    This article is an English version of an article which is originally in the Chinese language on echemi.com and is provided for information purposes only. This website makes no representation or warranty of any kind, either expressed or implied, as to the accuracy, completeness ownership or reliability of the article or any translations thereof. If you have any concerns or complaints relating to the article, please send an email, providing a detailed description of the concern or complaint, to service@echemi.com. A staff member will contact you within 5 working days. Once verified, infringing content will be removed immediately.

    Contact Us

    The source of this page with content of products and services is from Internet, which doesn't represent ECHEMI's opinion. If you have any queries, please write to service@echemi.com. It will be replied within 5 days.

    Moreover, if you find any instances of plagiarism from the page, please send email to service@echemi.com with relevant evidence.